Polymer Property : Izod Impact, Notched = 0.514 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 0.275 J/cm

@Thickness 3.17 mm
0.514 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® VB-5150GL PBT, 15% Glass Filled FR
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.275 J/cm

@Thickness 3.17 mm
0.514 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® GP-5000 PBT, Unreinforced
General PBT material that can be used for connectorsInformation provided by Samsung Cheil Industries.
Izod Impact, Notched 0.275 J/cm

@Thickness 3.17 mm
0.514 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® GP-5000 PBT, Unreinforced
General PBT material that can be used for connectorsInformation provided by Samsung Cheil Industries.
Izod Impact, Notched 0.275 J/cm

@Thickness 3.17 mm
0.514 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Infino® VB-5150GL PBT, 15% Glass Filled FR
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 0.275 J/cm

@Temperature 0.000 °C
0.514 ft-lb/in

@Temperature 32.0 °F
ASTM D256
SCG Chemicals EL-Proâ„¢ P401S Polypropylene Flat Yarn/Sheet
Key Characteristics: Excellent mechanical propertiesRecommended Applications:Stretch tape for jumbo woven sheetMonofilament for rope and sheetInformation provided by SCG Chemicals