Mechanical Properties Metric English Comments
Izod Impact, Notched 0.780 J/cm

@Thickness 3.17 mm
1.46 ft-lb/in

@Thickness 0.125 in
ASTM D256
LG Chemical MI-770 MIPS
Izod Impact, Notched 0.780 J/cm

@Thickness 6.35 mm
1.46 ft-lb/in

@Thickness 0.250 in
ASTM D256
LG Chemical 40 AF Flame Retardant HIPS
High impact, Safety standards: listed with UL CSA, and classified according to IEC 707, Meet requirements for flammability, mechanical and electrical properties, Applications include televisions, VT..
Izod Impact, Notched 0.780 J/cm

@Thickness 6.35 mm
1.46 ft-lb/in

@Thickness 0.250 in
ASTM D256
LG Chemical 501S-S HIPS
Self lubricant, Balanced mechanical properties, Good surface appearance with high gloss, Conforming to FDA CFR 177.1640, Excellent processability, Applications include refrigerator food holders, par..
Izod Impact, Notched 0.780 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
1.46 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
Asahi Kasei Xyron® X9102 Modified Polyphenylene Ether
High-Heat ResistantInformation provided by Asahi Kasei