Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LG Chemical 40 AF Flame Retardant HIPS

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Flame Retardant
Manufacturer LG Chemical
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical 40 AF Flame Retardant HIPS.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High impact, Safety standards: listed with UL CSA, and classified according to IEC 707, Meet requirements for flammability, mechanical and electrical properties, Applications include televisions, VTR, monitors, computers and other electrical electronic parts requiring flame retard
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Melt Flow 9.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
9.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 95
95
ASTM D785
Tensile Strength, Yield 26.5 MPa
3840 psi
50 mm/min; ASTM D638
Elongation at Break 60 %
60 %
50 mm/min; ASTM D638
Flexural Yield Strength 41.2 MPa
5980 psi
15 mm/min; ASTM D790
Flexural Modulus 2.20 GPa
319 ksi
15 mm/min; ASTM D790
Izod Impact, Notched 0.780 J/cm

@Thickness 6.35 mm
1.46 ft-lb/in

@Thickness 0.250 in
ASTM D256
1.13 J/cm

@Thickness 3.17 mm
2.12 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °C

@Thickness 12.7 mm
171 °F

@Thickness 0.500 in
Unannealed; ASTM D648
Vicat Softening Point 95.0 °C
203 °F
1000 g; ASTM D1525
Flammability, UL94 V-0
V-0
1/8 in
V-0
V-0
1/16 in
Electrical Properties Metric English Comments
Arc Resistance 60 - 120 sec
60 - 120 sec
UL Rating PLC 6 (60-120 sec)
Comparative Tracking Index 250 - 400 V
250 - 400 V
UL Rating PLC 2
Hot Wire Ignition, HWI 15 - 30 sec
15 - 30 sec
UL Rating PLC 3 (15-30 sec)
High Amp Arc Ignition, HAI >= 120 arcs
>= 120 arcs
UL Rating PLC 0 (>120 arcs)
High Voltage Arc-Tracking Rate, HVTR 10.0 - 25.4 mm/min
0.394 - 1.00 in/min
UL Rating PLC 1 (10-25.4 mm/min)
Descriptive Properties Value Comments
IEC 707 Flammability FVO mm/min.
1/16 in
Copyright © lookpolymers.com All Rights Reserved