Mechanical Properties Metric English Comments
Izod Impact, Notched 0.427 J/cm

@Temperature -20.0 °C
0.800 ft-lb/in

@Temperature -4.00 °F
1/8'' notched bar; ASTM D256
Ineos L12N-00 Polypropylene Impact Copolymer
This is a medium melt flow rate, nucleated impact copolymer polypropylene for injection molding and compounding applications. This material meets the requirements of the U.S. Food and Drug Administ..
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
0.800 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES HiFill® PA6 GF/M25 HS L BK 25% Glass/Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearance: BlackTPCI..
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
0.800 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES HiFill® PA6 GF/M30 HS BK 10/20% Glass/Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight and Mineral, 20% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat ..
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm,
Temperature -30.0 °C
0.800 ft-lb/in

@Thickness 0.125 in,
Temperature -22.0 °F
ASTM D256
Diamond Polymers Centrex® 835 Sheet Extrusion Grade
Centrex 835 resin is a low-gloss grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming applications. Centrex ..
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm,
Temperature -30.0 °C
0.800 ft-lb/in

@Thickness 0.125 in,
Temperature -22.0 °F
ASTM D256
Diamond Polymers DIAMALOY GLY 7510 High Heat ASA Weatherable Polymer
Diamaloy GLY 7510 resin is a high gloss, high heat and high impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. This product is rated f1 by UL and be customed..
Izod Impact, Notched 0.427 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
0.800 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D-256
Axiall 5009 Rigid PVC, Molding
Georgia Gulf 5009 is a type I, Grade I rigid vinyl injection molding compound designed for fittings and parts of similar confiation where maximum tensile strength and/or chemical resistance is requi..
Izod Impact, Notched 0.427 J/cm

@Temperature -30.0 °C
0.800 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Formosa Plastics Formolene® 6620A Impact Copolymer Polypropylene
High Impact Copolymer for Injection Molding Formolene® 6620A is a copolymer of polypropylene designed and formulated for injection molding applications including pails, crates and furniture. It con..
Izod Impact, Notched 0.427 J/cm

@Temperature -30.0 °C
0.800 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Formosa Plastics Formolene® 6630A Impact Copolymer Polypropylene
Impact Copolymer for Injection Molding Applications Formolene® 6630A is a high impact copolymer of polypropylene designed and formulated for injection-molded applications. It contains a unique comb..
Izod Impact, Notched 0.427 J/cm

@Thickness 3.17 mm,
Temperature -17.8 °C
0.800 ft-lb/in

@Thickness 0.125 in,
Temperature 0.000 °F
ASTM D256
Styron INSPIRE™ TF3800 Polypropylene
Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010