Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos L12N-00 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos L12N-00 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This is a medium melt flow rate, nucleated impact copolymer polypropylene for injection molding and compounding applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsAutomotiveConsumer productsHousewaresCompoundingBenefitsHigh impact resistanceHigh flexural modulusExcellent glossInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 75
75
ASTM D785
Tensile Strength, Yield 24.1 MPa

@Temperature 23.0 °C
3500 psi

@Temperature 73.4 °F
ASTM D638
Elongation at Break >= 200 %
>= 200 %
ASTM D638
Flexural Modulus 1.31 GPa

@Temperature 23.0 °C
190 ksi

@Temperature 73.4 °F
D790B
Izod Impact, Notched 0.427 J/cm

@Temperature -20.0 °C
0.800 ft-lb/in

@Temperature -4.00 °F
1/8'' notched bar; ASTM D256
1.17 J/cm

@Temperature 23.0 °C
2.20 ft-lb/in

@Temperature 73.4 °F
1/8'' notched bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 104 °C
220 °F
ASTM D648
Descriptive Properties Value Comments
Process Injection Molding
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution