Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.600 J/cm @Temperature -30.0 °C |
1.12 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS (Europe-Africa-Middle East) This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 23.0 °C |
1.12 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LATILUB 73/13-20T Polyoxymethylene Base (POM), 10% Mixed PTFE Self Lubricating Plastic
(Unverified D Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Izod Impact, Notched | >= 0.598 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
>= 1.12 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical LUPOL TE5208 PP+Rubber+MF, High Impact Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -30.0 °C |
1.12 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem UR9076LG PEI Standard flow mineral filled Polyetherimide Blend. Restricted sales to GE Specialty Film & Sheet.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -30.0 °C |
1.12 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® 6380U PBT+PET (Asia Pacific) XENOY 6380U is a 30% glass reinforced, UV stabilized grade, that combines high stiffness with improved ductility. The combination of mechanical properties at high and low temperatures and chemical r.. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -30.0 °C |
1.12 ft-lb/in @Temperature -22.0 °F |
ASTM Test |
Styrolution Terluran® GP-22 ABS Terluran GP-22 is an easy flowing grade of ABS for injection molding with high resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF and.. |
|||
Izod Impact, Notched | 0.598 J/cm @Thickness 6.35 mm |
1.12 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® VG-4920F ABS, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -30.0 °C |
1.12 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GTX GTX966 PPE+PA66 >PPE+PA66-I-TD10 |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 23.0 °C |
1.12 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GTX GTX966 PPE+PA66 (Asia Pacific) >PPE+PA66-I-TD10 |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -30.0 °C |
1.12 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GTX GTX966 PPE+PA66 (Asia Pacific) >PPE+PA66-I-TD10 |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 23.0 °C |
1.12 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GTX GTX966 PPE+PA66 (Europe-Africa-Middle East) >PPE+PA66-I-TD10 |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -30.0 °C |
1.12 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl GTX GTX966 PPE+PA66 (Europe-Africa-Middle East) >PPE+PA66-I-TD10 |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -30.0 °C |
1.12 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® X5630 PC+PET Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applicationsThis data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -40.0 °C |
1.12 ft-lb/in @Temperature -40.0 °F |
Practical Use (Water Absorption 2.1%); ASTM-D256 |
Toyobo GLAMIDE® NB-5620S Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 23.0 °C |
1.12 ft-lb/in @Temperature 73.4 °F |
Practical Use (Water Absorption 1.9%); ASTM-D256 |
Toyobo GLAMIDE® TY-502NZ 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -40.0 °C |
1.12 ft-lb/in @Temperature -40.0 °F |
Practical Use (Water Absorption 2.4%); ASTM-D256 |
Toyobo GLAMIDE® NB-1700 Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -40.0 °C |
1.12 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman DuraStar MN620 Polymer, Natural Applications:Blood therapyDrug deliveryIV componentsMedicalSurgical instrumentsKey Attributes:Chemical resistance to most medical solvents including lipids and IPAProduct Description: DuraStar Poly.. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -40.0 °C |
1.12 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Eastman Eastar BR203 Copolyester Eastar BR203 Copolyester contains a mold release additive. It has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilitie.. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 0.000 °C |
1.12 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTADIENE 0460 GF Acrylonitrile Butadiene Styrene, 30% Glass Filled ABS with 30% glass fiber reinforcementExcellent dimensional stability, low shrinkage, good impact resistanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 0.000 °C |
1.12 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTADIENE 0835 GF Acrylonitrile Butadiene Styrene, 17% Glass Filled ABS with 17% glass fiber reinforcementGood thermal resistance, good dimensional stability, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 0.000 °C |
1.12 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTADIENE 1016 T V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, with PBDE, high thermal resistance, good physical and mechanical characteristics, excellent processabilityInformation provided by Cossa Polim.. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 23.0 °C |
1.12 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Eastman TiGlaze SV Copolyester TiGLAZE SV copolyester is a specialty copolyester for the architectural glazing industry, designed to provide a unique balance of toughness, stiffness and material value. The material has a CC1 Ligh.. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 23.0 °C |
1.12 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTAPROP 1000 V2 K Flame Retardant Polypropylene PP copolymerFlame retardant class V2, PBDE free, good processability, good impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 23.0 °C |
1.12 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTAPROP H 0560 GF Polypropylene, 30% Glass Filled PP homopolymer 30% glass fiber reinforcedGood physical and mechanical characteristicsInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature 0.000 °C |
1.12 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTASTIR HI 0408 V0 Flame Retardant Polystyrene Flame retardant class V0, PBDE free, good impact resistance, good thermal resistance, high light resistance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 0.600 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
1.12 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilac ABS Acrylonitrile Butadiene Styrene |
|||
Izod Impact, Notched | 0.600 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
1.12 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilon G4-PC 20% GF Polycarbonate, 20% Glass Fiber Characteristics: 20% glass fibre filled, excellent mechanical properties |
|||
Izod Impact, Notched | 0.600 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
1.12 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epiryl G2 PPO 20GF Polyphenylene oxide, 20% Glass Fiber Characteristics: 20% glass fibre filled |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -20.0 °C |
1.12 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
Carmel Olefins CAPILENE® SE 50 E Polypropylene Impact Copolymer Description: CAPILENE® SE 50 E is a low melt flow rate impact copolymer intended for sheet extrusion. It exhibits excellent impact strength even at low temperatures, combined with good processabi.. |
|||
Izod Impact, Notched | 0.600 J/cm @Temperature -40.0 °C |
1.12 ft-lb/in @Temperature -40.0 °F |
Practical Use (Water Absorption 2.8%); ASTM-D256 |
Toyobo GLAMIDE® T-401 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |