Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.27 J/cm @Temperature -30.0 °C |
2.38 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Noble Polymers Regis™ 125098 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |
|||
Izod Impact, Notched | 1.27 J/cm @Temperature -20.0 °C |
2.39 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
PolyMirae Moplen EP200R Injection Molding Grade Polypropylene Moplen EP200R is the reactor TPO manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP200R is a super impact copolymer particularly suitable for injection molding of.. |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.39 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical AF342F ABS, Flame Retardant, High Flow Feature: Injection Molding, Flame Retardant, High FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided .. |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.39 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical BM662B ABS, Heat Resistance Feature: Blow Molding, Heat ResistanceApplication: Automotives Exterior Housing (Spoiler, Bumper Guard etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 31621-07-5Information provided by LG Chemica.. |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.39 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HIPS 60HRI PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: TV Sets, Tape Recorders, Vacuum Cleaner, Washing Machine, Air ConditionerCAS: 9003-55-8Information provided by LG Che.. |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.39 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HIPS 65IHE PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: Refrigerator Tray, Food Tray, Refrigerator Door LinerCAS: 9003-55-8Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.39 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LG709W ABS, Low Gloss, Heat Resistance Injection Molding, Low Gloss, Heat ResistanceApplication: Automobiles Interior Housing (Column Cover, Pilllars, Etc.)CAS No. 25120-20-1, 9003-56-9, 25747-74-7 and 9003-54-7Information provided by LG.. |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
2.39 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical RS656H ABS, Chemical Resistance to Cyclopentane Feature: Extrusion Molding, General Purpose, Chemical Resistance to CyclopentaneApplication: Refrigerator Inner LinerCAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.39 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical XR409HJ ABS, Heat Resistance, Curl Fit Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior & Exterior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by .. |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.39 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical XR474 ABS, Heat Resistance Feature: Injection Molding, Heat ResistanceApplication: Automotives Interior & Exterior HousingCAS No. 25120-20-1, 9003-56-9, 31621-07-5, and 9003-54-7Information provided by LG Chemical |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 3.17 mm |
2.38 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LG Chemical SG-950 Alphalac Polystyrene High strength, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include housing of electr.. |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
2.39 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical XR404HJ ABS, Heat Resistance, Curl Fit Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by LG Chemica.. |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 6.35 mm |
2.39 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® HP-0500 ABS, Unreinforced Heat Resistant ABS material that can mainly be used for the exterior material of household appliances etc.Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 3.17 mm |
2.39 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® HP-0500 ABS, Unreinforced Heat Resistant ABS material that can mainly be used for the exterior material of household appliances etc.Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 3.17 mm |
2.39 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® MKD-1016 PA, 55% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 6.35 mm |
2.39 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® BF-0370 MABS, Unreinforced Scratch Resistant Scratch resistant material that is used in the exterior of electric products and household appliancesInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 6.35 mm |
2.39 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® HG-0760LT ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 6.35 mm |
2.39 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® NT-7310 ABS, Unreinforced FR Flame-retardant ABS that can be used in printer frames etc.Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
2.39 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Samsung Cheil Industries Starex® SR-0330M ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 6.35 mm |
2.39 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® HP-0500 ABS, Unreinforced Heat Resistant ABS material that can mainly be used for the exterior material of household appliances etc.Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 3.17 mm |
2.39 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® MKD-1016 PA, 55% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 6.35 mm |
2.39 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® BF-0370 MABS, Unreinforced Scratch Resistant Scratch resistant material that is used in the exterior of electric products and household appliancesInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 6.35 mm |
2.39 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® HF-0690M ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 6.35 mm |
2.39 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Starex® HG-0760LT ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
2.39 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Samsung Cheil Industries Starex® SR-0330M ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 1.27 J/cm @Temperature 0.000 °C |
2.39 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SCG Chemicals EL-Leneâ„¢ H5211PBR High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stabilityRecommended Applications: Non pressure pipes, co-extruded pipes as the inner layerInformation provided by SCG Chemicals |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 6.40 mm |
2.39 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron IMC25 ABS-PC Alloy Medium FlowInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 3.20 mm |
2.39 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron KU670M ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 3.20 mm |
2.39 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Bhansali Engineering Abstron KU670M ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Izod Impact, Notched | 1.27 J/cm @Thickness 6.40 mm |
2.39 ft-lb/in @Thickness 0.252 in |
ASTM D256 |
Bhansali Engineering Abstron IMC25 ABS-PC Alloy Medium FlowInformation provided by Bhansali |