Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LG Chemical HIPS 60HRI PS, Impact Modified

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer LG Chemical
Trade Name HIPS
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical HIPS 60HRI PS, Impact Modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: TV Sets, Tape Recorders, Vacuum Cleaner, Washing Machine, Air ConditionerCAS: 9003-55-8Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
ASTM D792
Maximum Moisture Content 0.010
0.010
Injection Molding
Melt Flow 6.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
6.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
15 g/10 min

@Load 3.80 kg,
Temperature 230 °C
15 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
65 g/10 min

@Load 10.0 kg,
Temperature 220 °C
65 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 99
99
ASTM D785
Tensile Strength, Yield 26.5 MPa

@Thickness 3.20 mm
3840 psi

@Thickness 0.126 in
50mm/min; ASTM D638
Elongation at Break 62 %

@Thickness 3.20 mm
62 %

@Thickness 0.126 in
50mm/min; ASTM D638
Elongation at Yield >= 5.0 %

@Thickness 3.20 mm
>= 5.0 %

@Thickness 0.126 in
50mm/min; ASTM D638
Tensile Modulus 1.78 GPa

@Thickness 3.20 mm
259 ksi

@Thickness 0.126 in
1mm/min; ASTM D638
Flexural Yield Strength 42.2 MPa

@Thickness 3.20 mm
6120 psi

@Thickness 0.126 in
15mm/min; ASTM D790
Flexural Modulus 2.13 GPa

@Thickness 3.20 mm
309 ksi

@Thickness 0.126 in
15mm/min; ASTM D790
Izod Impact, Notched 0.490 J/cm

@Thickness 6.40 mm,
Temperature -30.0 °C
0.918 ft-lb/in

@Thickness 0.252 in,
Temperature -22.0 °F
ASTM D256
0.588 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
1.10 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
0.883 J/cm

@Thickness 6.40 mm,
Temperature 23.0 °C
1.65 ft-lb/in

@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
1.27 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
2.39 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °C

@Thickness 6.40 mm
196 °F

@Thickness 0.252 in
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C

@Thickness 6.40 mm
180 °F

@Thickness 0.252 in
Unannealed; ASTM D648
Vicat Softening Point 90.0 °C

@Load 5.00 kg
194 °F

@Load 11.0 lb
50°C/h; ASTM D1525
UL RTI, Electrical 50.0 °C

@Thickness >=1.50 mm
122 °F

@Thickness >=0.0591 in
50.0 °C

@Thickness >=3.00 mm
122 °F

@Thickness >=0.118 in
UL RTI, Mechanical with Impact 50.0 °C

@Thickness >=1.50 mm
122 °F

@Thickness >=0.0591 in
50.0 °C

@Thickness >=3.00 mm
122 °F

@Thickness >=0.118 in
UL RTI, Mechanical without Impact 50.0 °C

@Thickness >=1.50 mm
122 °F

@Thickness >=0.0591 in
50.0 °C

@Thickness >=3.00 mm
122 °F

@Thickness >=0.118 in
Flammability, UL94 HB

@Thickness >=1.50 mm
HB

@Thickness >=0.0591 in
HB

@Thickness >=3.00 mm
HB

@Thickness >=0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
Dielectric Strength 42.0 kV/mm
1070 kV/in
Arc Resistance 120 - 180 sec
120 - 180 sec
ASTM D495
Hot Wire Ignition, HWI 7.0 - 15 sec

@Thickness >=1.50 mm
7.0 - 15 sec

@Thickness >=0.0591 in
15 - 30 sec

@Thickness >=3.00 mm
15 - 30 sec

@Thickness >=0.118 in
High Amp Arc Ignition, HAI 60 - 120 arcs

@Thickness 1.50 mm
60 - 120 arcs

@Thickness 0.0591 in
>= 120 arcs

@Thickness 3.00 mm
>= 120 arcs

@Thickness 0.118 in
High Voltage Arc-Tracking Rate, HVTR 25.4 - 50.0 mm/min
1.00 - 1.97 in/min
Processing Properties Metric English Comments
Rear Barrel Temperature 170 - 190 °C
338 - 374 °F
Injection Molding
Middle Barrel Temperature 180 - 200 °C
356 - 392 °F
Injection Molding
Front Barrel Temperature 190 - 210 °C
374 - 410 °F
Injection Molding
Nozzle Temperature 190 - 220 °C
374 - 428 °F
Injection Molding
Melt Temperature 190 - 220 °C
374 - 428 °F
Injection Molding
Mold Temperature 40.0 - 70.0 °C
104 - 158 °F
Injection Molding
Drying Temperature 80.0 °C
176 °F
Injection Molding
Dry Time 2.00 - 4.00 hour
2.00 - 4.00 hour
Injection Molding
Back Pressure 29.4 - 58.8 MPa
4260 - 8530 psi
Injection Molding
Screw Speed 30 - 60 rpm
30 - 60 rpm
Injection Molding