Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.00 J/cm @Temperature -30.0 °C |
1.87 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc.. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 23.0 °C |
1.87 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® XCM851 PC+ABS (Europe-Africa-Middle East) High heat PC/ABS blend offering high modulus / low CTE and good practical impactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -30.0 °C |
1.87 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -30.0 °C |
1.87 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® SLX1431T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa-Middle .. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -30.0 °C |
1.87 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -30.0 °C |
1.87 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® SLX1431T PC Copolymer (Asia Pacific) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -30.0 °C |
1.87 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® SLX2431D PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in diffusion colors.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 1.00 J/cm @Thickness 3.20 mm, Temperature 0.000 °C |
1.87 ft-lb/in @Thickness 0.126 in, Temperature 32.0 °F |
ASTM D256 |
Mapal Plastics Maplon Type S Polypropylene Sheet Properties: Low stress whitening, Suitable for die cutting, Corona treated on both sides for offset and screen printingApplications: Stationery, Packaging, House-hold productsand printed items |
|||
Izod Impact, Notched | >= 1.00 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
>= 1.87 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Kingfa LONOY 1600 PC/PBT Alloy Features:Excellent balance propertiesGood weather resistanceGood size stabilitySmooth surfaceUniform colorApplications:Injection moldingAutomobile bumperAutomobile interior/exterior trim partsBusine.. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -29.0 °C |
1.87 ft-lb/in @Temperature -20.2 °F |
3.2 mm (0.125 in) notch |
Kraton® FG1901 + PBT blend (30/70), Oven Aged Oven aged at 150°C (°F) for 2 hours. KRATON polymers are block segments of styrene and rubber monomers (A-B, A-B-A, or [A-B]n). The KRATON G series are second generation block polymers in whi.. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -30.0 °C |
1.87 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Xylex X8303CL PC+POLYESTER PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling.This data was supplied by SABIC-IP for the Americ.. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -18.0 °C |
1.87 ft-lb/in @Temperature -0.400 °F |
ASTM Test |
Styrolution Terluran® GP-22 ABS Terluran GP-22 is an easy flowing grade of ABS for injection molding with high resistance to impact and heat deflection.Information provided by STYROLUTION, which is a joint venture between BASF and.. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 23.0 °C |
1.87 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl FXN2090H PPE+HIPS (Europe-Africa-Middle East) Noryl* FXN2090H resin is an unfilled, injection moldable grade. Designed for exceptionally high gloss and improved pencil hardness vs. standard Noryl grades, FXN2090H resin uses non-halogenated FR a.. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 23.0 °C |
1.87 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTABLEND 0840 GF Polycarbonate ABS Blend, 20% Glass Filled Polycarbonate and Acrylonitrile Butadiene Styrene blend with 20% glass fiber reinforcementHigh dimensional stability, high stiffnessInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 0.000 °C |
1.87 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTACARB 0820 GF V0-5V Flame Retardant Polycarbonate Polycarbonate with 10% glass fiber reinforcementFlame retardant class V0, PBDE free, high stiffness, high dimensional stability, good melt flow, good processability, good light resistanceInformation.. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 0.000 °C |
1.87 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTADIENE 0615 HHT Acrylonitrile Butadiene Styrene ABS with very high heat resistanceGood impact resistance, stiff, excellent surface appearance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 0.000 °C |
1.87 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTADIENE 0815 HHT Acrylonitrile Butadiene Styrene ABS with very high heat resistanceGood melt flow rate, good impact resistance, excellent surface appearance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 23.0 °C |
1.87 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTADIENE 1030 T V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, high thermal resistance, good impact resistance, high gloss, good light resistance, good processabilityInformation provided by Cos.. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 23.0 °C |
1.87 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTADIENE 1218 HT V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, PBDE free, good impact resistance, excellent processability, good surface appearance, high thermal resistanceInformation provided by Cossa Po.. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 23.0 °C |
1.87 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTAPROP H 0540 GFC Polypropylene, 20% Glass Filled PP homopolymer 20% chemically coupled glass fiber reinforcedInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 0.000 °C |
1.87 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTAPROP H 0560 HFC Polypropylene, 30% Glass Filled PP homopolymer 30% chemically coupled glass fiber reinforcedGood stiffness, excellent impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 23.0 °C |
1.87 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTAPROP H 1660 GFC Polypropylene, 30% Glass Filled PP homopolymer 30% chemically coupled glass fiber reinforcedHigh melt flow rate, excellent impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 23.0 °C |
1.87 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTASTIR HI 10 V0 Flame Retardant Polystyrene Flame retardant class V0, with PBDE, for injection molding or extrusionInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 1.00 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
1.87 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epicarb PC BLACK IQ Polycarbonate Characteristics: good fluidity, good impact, industrial quality |
|||
Izod Impact, Notched | 1.00 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
1.87 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilon G2-PC 10% GF Polycarbonate, 10% Glass Fiber Characteristics: 10% glass fibre filled, good mechanical properties |
|||
Izod Impact, Notched | 1.00 - 1.80 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
1.87 - 3.37 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256, ISO 180/4a |
EPICHEM Epilon PC UVR Polycarbonate, High Impact Characteristics: high fluidity, high impact, UV resistant |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -20.0 °C |
1.87 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
Carmel Olefins CAPILENE® TR 50 Polypropylene Impact Copolymer Description: CAPILENE® TR 50 is a medium melt flow rate heterophasic copolymer with very high impact strength, even at low temperature, designed for injection molding. This grade combines good pr.. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature -20.0 °C |
1.87 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
Carmel Olefins CAPILENE® TT 75 AV Polypropylene Impact Copolymer Description: CAPILENE® TT 75 AV is a nucleated, controlled rheology heterophasic copolymer designed for injection molding. It is characterized by excellent impact strength, even at low temperatur.. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 23.0 °C |
1.87 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Braskem CP 141 Injection Molding Polypropylene Description: CP 141 is a high melt flow rate heterophasic copolymer specially designed to achieve high productivity on thin-walled parts with very easy mould filling and high speed injection mouldin.. |
|||
Izod Impact, Notched | 1.00 J/cm @Temperature 23.0 °C |
1.87 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LATI LASULF G/30 30% Glass Reinforced Polysulfone (PSU)
(Unverified Data**) Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi.. |