Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Carmel Olefins CAPILENE® TT 75 AV Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Carmel Olefins
Trade Name CAPILENE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Carmel Olefins CAPILENE® TT 75 AV Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: CAPILENE® TT 75 AV is a nucleated, controlled rheology heterophasic copolymer designed for injection molding. It is characterized by excellent impact strength, even at low temperature, good flow characteristics and antistatic additive.Applications: CAPILENE® TT 75 AV is suitable for automotive articles, heavy duty technical parts, household articles, shelves, cabinets, garden furniture, crates, large containers, pails and tool boxes.Information provided by Carmel Olefins.
Physical Properties Metric English Comments
Melt Flow 25 g/10 min

@Load 2.16 kg,
Temperature 230 °C
25 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 18.0 MPa
2610 psi
50 mm/min; ASTM D638
Elongation at Yield 8.0 %
8.0 %
50 mm/min; ASTM D638
Flexural Modulus 0.850 GPa
123 ksi
ASTM D790
Izod Impact, Notched 1.00 J/cm

@Temperature -20.0 °C
1.87 ft-lb/in

@Temperature -4.00 °F
ASTM D256
5.00 J/cm

@Temperature 23.0 °C
9.37 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C
167 °F
ASTM D648
Vicat Softening Point 140 °C

@Load 1.02 kg
284 °F

@Load 2.25 lb
ASTM D1525