Mechanical Properties Metric English Comments
Izod Impact, Notched 1.90 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
3.56 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 87180 Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te..
Izod Impact, Notched 1.90 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
3.56 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion 87759 Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: Finished part testing is required for ASTM E-84 certification. Note: The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by Po..
Izod Impact, Notched 1.90 J/cm

@Thickness 3.20 mm,
Temperature 0.000 °C
3.56 ft-lb/in

@Thickness 0.126 in,
Temperature 32.0 °F
ISO 180/4A
Polimeri Europa Sinkral® B 532/E ABS Resin
Sinkral B 532/E is an extrusion grade, which combines high toughness with good rigidity. Its rheological characteristics and good thermal stability are required for the production of large extruded ..
Izod Impact, Notched 1.90 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
3.56 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ISO 180/4A
Polimeri Europa Sinkral® E 332 ABS Resin
Sinkral E 332 is a medium heat injection molding grade offering good flow and good impact resistance together with an excellent thermal stability during processing. Designation: Thermoplastic ISO 2..
Izod Impact, Notched 1.90 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
3.56 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ISO 180/4A
Polimeri Europa Sinkral® F 332 ABS Resin
Sinkral F 332 is a general purpose injection molding grade which combines excellent thermal stability during processing with a good balance between flow and impact characteristics. Designation: Ther..
Izod Impact, Notched 1.90 J/cm

@Thickness 3.18 mm,
Temperature -20.0 °C
3.56 ft-lb/in

@Thickness 0.125 in,
Temperature -4.00 °F
Injection Molded; ASTM D256A
PolyOne Edgetek® XT XT-100-BU03 Black Polycarbonate + PBT (PC+PBT)
EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen..
Izod Impact, Notched 1.90 J/cm

@Temperature -29.0 °C
3.56 ft-lb/in

@Temperature -20.2 °F
ASTM D256
Styron MAGNUMâ„¢ 1250 BG Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: High Impact, High Heat, Blow Molding ABSInformation provided by Styron
Izod Impact, Notched 1.90 J/cm

@Temperature 23.0 °C
3.56 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Styron MAGNUMâ„¢ 3325 SLG Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: Super Low Gloss, Medium Heat, Medium Impact ABS resin for injection molded automotive interior trim applications Magnum 3325 SLG can achieve 60° Gardner gloss levels below 2.0 with low ..
Izod Impact, Notched 1.90 J/cm

@Temperature 23.0 °C
3.56 ft-lb/in

@Temperature 73.4 °F
Absolute Drying; ASTM-D256
Toyobo GLAMIDE® T-403 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 1.90 J/cm

@Temperature 23.0 °C
3.56 ft-lb/in

@Temperature 73.4 °F
Practical Use (Water Absorption 0.8%); ASTM-D256
Toyobo GLAMIDE® T-663G50A MXD66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 1.90 J/cm

@Temperature -40.0 °C
3.56 ft-lb/in

@Temperature -40.0 °F
Practical Use (Water Absorption 1.6%); ASTM-D256
Toyobo GLAMIDE® TY-181GC Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 1.90 J/cm

@Temperature 23.0 °C
3.56 ft-lb/in

@Temperature 73.4 °F
Practical Use (Water Absorption 2.8%); ASTM-D256
Toyobo GLAMIDE® T-401 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Izod Impact, Notched 1.90 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
3.56 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
PolyOne Geon™ Vinyl Rigid Extrusion L6181 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Izod Impact, Notched 1.90 J/cm

@Temperature -20.0 °C
3.56 ft-lb/in

@Temperature -4.00 °F
ASTM D256
LATI LARIL 13-V1 Polyphenylene Oxide (PPOm) (UL94V-1)  (discontinued **)
Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most ..