Izod Impact, Notched 11.2 J/cm

@Thickness 3.17 mm
21.0 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Axiall 3121 Rigid PVC, Extrusion
Georgia Gulf 3121 is an exterior grade powder compound formulated for processing applications requiring high production output rate. Having excellent weatherability and impact strength, 3121 is sui..
Izod Impact, Notched 11.2 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
21.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Axiall 7055 Rigid PVC, Extrusion
Georgia Gulf 7055 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: WeatherabilityChemicalDurabilityEase of ProcessingToughnessInformat..