Material Notes:
Georgia Gulf 7055 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: WeatherabilityChemicalDurabilityEase of ProcessingToughnessInformation provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.43 g/cc
1.43 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 106
106
ASTM D-785
Hardness, Shore D 80
80
ASTM D-2240
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D-638
Tensile Modulus 2.58 GPa
374 ksi
ASTM D-638
Flexural Strength 75.8 MPa
11000 psi
ASTM D-790
Flexural Modulus 2.73 GPa
396 ksi
ASTM D-790
Izod Impact, Notched 8.54 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
16.0 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D-256
11.2 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
21.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Tensile Impact Strength 168 kJ/m²
80.0 ft-lb/in²
ASTM D-1822
Dart Drop Total Energy 49.1 J/cm
0.0920 ft-lb/mil
23°C, C.125 Tup, Method A; ASTM D-4226
155 J/cm
0.290 ft-lb/mil
H.25 Tup, Method A; ASTM D-4226
Thermal Properties Metric English Comments
CTE, linear 64.8 µm/m-°C

@Temperature 20.0 °C
36.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 71.1 °C
160 °F
ASTM D-648
Processing Properties Metric English Comments
Melt Temperature 182 °C
360 °F
Descriptive Properties Value Comments
Cell Classification 14433233
ASTM D-4216
Users viewing this material also viewed the following: