Polymer Property : Izod Impact, Notched = 12.3 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 12.3 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
23.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Axiall 9246 Rigid PVC, Molding
Georgia Gulf 9246 is a high impact compound suitable for food packaging.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Izod Impact, Notched 12.3 J/cm

@Thickness 3.17 mm
23.0 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Axiall 5055 Rigid PVC, Extrusion, White
Georgia Gulf 5055 White is a special purpose rigid PVC compound designed for applications requiring the following properties: ToughnessUL RatingEase of ProcessingDurabilityChemical ResistantOutdoor..
Izod Impact, Notched 12.3 J/cm

@Thickness 3.17 mm
23.0 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Axiall 7555 Rigid PVC, Extrusion, Natural
Georgia Gulf 7555 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: ToughnessDurabilityUL RatingChemical ResistanceEase of ProcessingIn..
Izod Impact, Notched 12.3 J/cm

@Thickness 3.17 mm
23.0 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Axiall 7555 Rigid PVC, Extrusion, White
Georgia Gulf 7555 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: ToughnessDurabilityUL RatingChemical ResistanceEase of ProcessingIn..
Izod Impact, Notched 12.3 J/cm

@Thickness 3.17 mm
23.0 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Axiall 5055 Rigid PVC, Extrusion, Natural
Georgia Gulf 5055 is a special purpose rigid PVC compound designed for applications requiring the following properties: ToughnessUL RatingEase of ProcessingDurabilityChemical RetardantInformation p..