Axiall 9246 Rigid PVC, Molding

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 9246 Rigid PVC, Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf 9246 is a high impact compound suitable for food packaging.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.7 MPa
5900 psi
ASTM D-638
Tensile Modulus 2.39 GPa
346 ksi
ASTM D-638
Flexural Strength 65.5 MPa
9500 psi
ASTM D-790
Flexural Modulus 2.17 GPa
315 ksi
ASTM D-790
Izod Impact, Notched 9.08 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
17.0 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D-256
12.3 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
23.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Tensile Impact Strength 202 kJ/m²
96.0 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 62.00 °C
143.6 °F
annealed; ASTM D-648
Optical Properties Metric English Comments
Haze 5.0 %

@Thickness 3.17 mm
5.0 %

@Thickness 0.125 in
pressed plaque; ASTM D-1003-61
Transmission, Visible 75 %

@Thickness 3.17 mm
75 %

@Thickness 0.125 in
pressed plaque; ASTM D-1003-61
Descriptive Properties Value Comments
Equilibrium Torque, meter-grams 1350
Brabender Plastograph, No. 6 Roller Head, 190°C Bath, 57-g. Charge; 60/43 rpm
Stability Time, minutes 33