Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.65 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
4.96 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical AF342T ABS, Flame Retardant, High Impact Feature: Injection Molding, Flame Retardant, High ImpactApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provide.. |
|||
Izod Impact, Notched | 2.65 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
4.96 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HF380G ABS, High Flow Feature: Injection Molding, High FlowApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 2.65 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
4.96 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HF380U ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 2.65 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
4.96 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LG749W ABS, Low Gloss, Heat Resistance Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automotive Interior Housing (Glove Cover, Door S/W Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by.. |
|||
Izod Impact, Notched | 2.65 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
4.96 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical PI642G ABS, General Purpose, High Modulus Feature: Extrusion Molding, General Purpose, High ModulusApplication: Pipe fittingCAS No. 9003-56-9Information provided by LG Chemical |
|||
Izod Impact, Notched | 2.65 J/cm @Thickness 6.35 mm |
4.96 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® HR-1008B PC/ABS, Unreinforced PC/ABS material that can be used for hand phone and car phoneInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.65 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
4.96 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D256 |
Samsung Cheil Industries Starex® MP-0670 ABS, Metal Plating Grade Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.65 J/cm @Thickness 3.17 mm |
4.96 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® QU-0191S ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.65 J/cm @Thickness 6.35 mm |
4.96 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Samsung Cheil Industries Infino® HR-1008B PC/ABS, Unreinforced PC/ABS material that can be used for hand phone and car phoneInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.65 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
4.96 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D256 |
Samsung Cheil Industries Starex® MP-0670 ABS, Metal Plating Grade Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.65 J/cm @Thickness 3.17 mm |
4.96 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® QU-0191S ABS, Unreinforced Extrusion Grade Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 2.65 J/cm @Temperature 0.000 °C |
4.96 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SCG Chemicals EL-Leneâ„¢ H1000PBL High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, good resistance to weathering, good balance of MRS and SCGRecommended Applications: Water pressure pipes and stripe lines for PE100 pi.. |
|||
Izod Impact, Notched | 2.65 J/cm @Temperature 0.000 °C |
4.96 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SCG Chemicals EL-Leneâ„¢ H1000PYL High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, good resistance to weatheringRecommended Applications: Stripe lines for PE100 pipe, non pressure pipesCertification: Certified by LNE.. |
|||
Izod Impact, Notched | 2.65 J/cm @Temperature 23.0 °C |
4.96 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
E-Polymers SEPAZ® LH50 PP Homopolymer LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Izod Impact, Notched | 2.65 J/cm @Temperature -30.0 °C |
4.96 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
E-Polymers SEPAZ® LH50 PP Homopolymer LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Izod Impact, Notched | 2.65 J/cm @Temperature 23.0 °C |
4.96 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
E-Polymers SEPAZ® LA40 PA66 LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Izod Impact, Notched | 2.65 J/cm @Temperature -30.0 °C |
4.96 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
E-Polymers SEPAZ® LA40 PA66 LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Izod Impact, Notched | 2.65 J/cm @Temperature 23.0 °C |
4.96 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
E-Polymers SEPAZ® LH60 PP Homopolymer LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Izod Impact, Notched | 2.65 J/cm @Temperature -30.0 °C |
4.96 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
E-Polymers SEPAZ® LH60 PP Homopolymer LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |