Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 4.96 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.65 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
4.96 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical AF342T ABS, Flame Retardant, High Impact
Feature: Injection Molding, Flame Retardant, High ImpactApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provide..
Izod Impact, Notched 2.65 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
4.96 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical HF380G ABS, High Flow
Feature: Injection Molding, High FlowApplication: Electric & Electronic Products)CAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 2.65 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
4.96 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical HF380U ABS, High Flow
Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous Goods)CAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 2.65 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
4.96 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical LG749W ABS, Low Gloss, Heat Resistance
Feature: Injection Molding, Low Gloss, Heat ResistanceApplication: Automotive Interior Housing (Glove Cover, Door S/W Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by..
Izod Impact, Notched 2.65 J/cm

@Thickness 3.20 mm,
Temperature 23.0 °C
4.96 ft-lb/in

@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
LG Chemical PI642G ABS, General Purpose, High Modulus
Feature: Extrusion Molding, General Purpose, High ModulusApplication: Pipe fittingCAS No. 9003-56-9Information provided by LG Chemical
Izod Impact, Notched 2.65 J/cm

@Thickness 6.35 mm
4.96 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Infino® HR-1008B PC/ABS, Unreinforced
PC/ABS material that can be used for hand phone and car phoneInformation provided by Samsung Cheil Industries.
Izod Impact, Notched 2.65 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
4.96 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
Samsung Cheil Industries Starex® MP-0670 ABS, Metal Plating Grade
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.65 J/cm

@Thickness 3.17 mm
4.96 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® QU-0191S ABS, Unreinforced Extrusion Grade
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.65 J/cm

@Thickness 6.35 mm
4.96 ft-lb/in

@Thickness 0.250 in
ASTM D256
Samsung Cheil Industries Infino® HR-1008B PC/ABS, Unreinforced
PC/ABS material that can be used for hand phone and car phoneInformation provided by Samsung Cheil Industries.
Izod Impact, Notched 2.65 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
4.96 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256
Samsung Cheil Industries Starex® MP-0670 ABS, Metal Plating Grade
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.65 J/cm

@Thickness 3.17 mm
4.96 ft-lb/in

@Thickness 0.125 in
ASTM D256
Samsung Cheil Industries Starex® QU-0191S ABS, Unreinforced Extrusion Grade
Information provided by Samsung Cheil Industries.
Izod Impact, Notched 2.65 J/cm

@Temperature 0.000 °C
4.96 ft-lb/in

@Temperature 32.0 °F
ASTM D256
SCG Chemicals EL-Leneâ„¢ H1000PBL High Density Polyethylene Pipe Resin
Key Characteristics: Good processing, high thermal stability, good resistance to weathering, good balance of MRS and SCGRecommended Applications: Water pressure pipes and stripe lines for PE100 pi..
Izod Impact, Notched 2.65 J/cm

@Temperature 0.000 °C
4.96 ft-lb/in

@Temperature 32.0 °F
ASTM D256
SCG Chemicals EL-Leneâ„¢ H1000PYL High Density Polyethylene Pipe Resin
Key Characteristics: Good processing, high thermal stability, good resistance to weatheringRecommended Applications: Stripe lines for PE100 pipe, non pressure pipesCertification: Certified by LNE..
Izod Impact, Notched 2.65 J/cm

@Temperature 23.0 °C
4.96 ft-lb/in

@Temperature 73.4 °F
ASTM D256
E-Polymers SEPAZ® LH50 PP Homopolymer LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Izod Impact, Notched 2.65 J/cm

@Temperature -30.0 °C
4.96 ft-lb/in

@Temperature -22.0 °F
ASTM D256
E-Polymers SEPAZ® LH50 PP Homopolymer LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Izod Impact, Notched 2.65 J/cm

@Temperature 23.0 °C
4.96 ft-lb/in

@Temperature 73.4 °F
ASTM D256
E-Polymers SEPAZ® LA40 PA66 LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Izod Impact, Notched 2.65 J/cm

@Temperature -30.0 °C
4.96 ft-lb/in

@Temperature -22.0 °F
ASTM D256
E-Polymers SEPAZ® LA40 PA66 LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Izod Impact, Notched 2.65 J/cm

@Temperature 23.0 °C
4.96 ft-lb/in

@Temperature 73.4 °F
ASTM D256
E-Polymers SEPAZ® LH60 PP Homopolymer LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Izod Impact, Notched 2.65 J/cm

@Temperature -30.0 °C
4.96 ft-lb/in

@Temperature -22.0 °F
ASTM D256
E-Polymers SEPAZ® LH60 PP Homopolymer LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Copyright © lookpolymers.com All Rights Reserved