Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.78 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
5.20 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8010 Availability: North AmericaForms: PelletsProcessing Method: Extrusion Blow Molding and Sheet ExtrusionInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 2.78 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
5.20 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS 8002 Availability: North AmericaForms: PelletsFeatures: High Heat ResistanceProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 2.78 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
5.20 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Luriblend® ABS X MB Availability: North AmericaForms: PelletsAdditive: Silicone LubricantFeatures: General Purpose and LubricatedInformation provided by TP Composites, Inc. |