Polymer Property : Izod Impact, Notched = 5.20 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 2.78 J/cm

@Thickness 3.17 mm,
Temperature 0.000 °C
5.20 ft-lb/in

@Thickness 0.125 in,
Temperature 32.0 °F
ASTM D256
Techmer ES Plastiblend® ABS 8010
Availability: North AmericaForms: PelletsProcessing Method: Extrusion Blow Molding and Sheet ExtrusionInformation provided by TP Composites, Inc.
Izod Impact, Notched 2.78 J/cm

@Thickness 3.17 mm,
Temperature 0.000 °C
5.20 ft-lb/in

@Thickness 0.125 in,
Temperature 32.0 °F
ASTM D256
Techmer ES Plastiblend® ABS 8002
Availability: North AmericaForms: PelletsFeatures: High Heat ResistanceProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Izod Impact, Notched 2.78 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
5.20 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Luriblend® ABS X MB
Availability: North AmericaForms: PelletsAdditive: Silicone LubricantFeatures: General Purpose and LubricatedInformation provided by TP Composites, Inc.