Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.50 J/cm @Temperature 23.0 °C |
6.56 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CY5105 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applicationsThis data was supplied by SABIC-IP .. |
|||
Izod Impact, Notched | 3.50 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
6.56 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
Kingfa MAC-751 HF PC/ABS Alloy Features:Excellent balance propertiesSuper high impact strengthGood electro-plating propertiesGood processing propertiesGood glossApplications:Injection moldingAutomobile instrument panelElectrical .. |
|||
Izod Impact, Notched | 3.50 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
6.56 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
Kingfa MAC-751 PC/ABS Alloy Features:Excellent balance propertiesSuper high impact strengthGood electro-plating propertiesGood processing propertiesGood glossApplications:Injection moldingAutomobile instrument panelElectrical .. |
|||
Izod Impact, Notched | 3.50 J/cm @Temperature -30.0 °C |
6.56 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Asia Pacific) XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Asia Pacific reg.. |
|||
Izod Impact, Notched | 3.50 J/cm @Temperature -30.0 °C |
6.56 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Europe-Africa-Middle East) XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Europe-Africa-Mi.. |
|||
Izod Impact, Notched | 3.50 J/cm @Temperature 23.0 °C |
6.56 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTADIENE 2506 Acrylonitrile Butadiene Styrene ABS for sheet and profile extrusionHigh impact resistance, excellent heat resistance, excellent dimensional stability and processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 3.50 J/cm @Temperature 0.000 °C |
6.56 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTADIENE 3008 MT Acrylonitrile Butadiene Styrene ABS with very high impact resistanceHigh impact resistance at low temperature, medium heat resistance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 3.50 J/cm @Temperature 23.0 °C |
6.56 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTADIENE 3015 MT Acrylonitrile Butadiene Styrene ABSMedium thermal resistance, high impact resistance at low temperature, good melt flow rate, high gloss, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 3.50 J/cm @Temperature 23.0 °C |
6.56 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTADIENE 3510 HT Acrylonitrile Butadiene Styrene ABS with very high impact resistanceHigh impact resistance at low temperature, high heat resistance, good processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 3.50 J/cm @Temperature 23.0 °C |
6.56 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
Cossa Polimeri ESTADIENE 3520 Acrylonitrile Butadiene Styrene ABS with high impact resistanceHigh melt flow rate, high impact resistance at low temperature, excellent processability and surface appearanceInformation provided by Cossa Polimeri S.r.l. |
|||
Izod Impact, Notched | 3.50 J/cm @Temperature 0.000 °C |
6.56 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTADIENE CR 1 Acrylonitrile Butadiene Styrene ABS for chrome platingGood melt flow rate, high impact resistance at low temperature, high gloss, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |