Mechanical Properties Metric English Comments
Izod Impact, Notched 2.94 J/cm

@Thickness 6.35 mm,
Temperature 22.8 °C
5.50 ft-lb/in

@Thickness 0.250 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Elastoblend® PC E IM
Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact Modified and High ViscosityProcessing Method: ExtrusionInformation provided by TP Composites, Inc.
Izod Impact, Notched 2.94 J/cm

@Thickness 3.17 mm,
Temperature 72.8 °C
5.50 ft-lb/in

@Thickness 0.125 in,
Temperature 163 °F
ASTM D256
Techmer ES Luriblend® PA4/6 HS TL15
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (15%)Features: Heat Stabilized and LubricatedUL File Number: E157318Information provided by TP Composites, Inc...
Izod Impact, Notched 2.94 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
5.50 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Luriblend® PA4/6 TL15 HS
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and PTFE Lubricant (15%)Features: Heat Stabilized, Low Friction, Good Wear Resistance and LubricatedInformation provided by TP Com..
Izod Impact, Notched 2.94 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
5.50 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
Techmer ES Plastiblend® PC/PBT IM 5220 BK