Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 3.80 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
7.12 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Rigid Extrusion 87570 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Izod Impact, Notched | 3.80 J/cm @Temperature -30.0 °C |
7.12 ft-lb/in @Temperature -22.0 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® CP8930 PC+ABS (Europe-Africa-Middle East) High heat, PC/ABS for automotive electro plating applications, excellent balance in flow/impactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 3.80 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
7.12 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Kingfa JH950-502 Low-temperature Resistant & Flame Retardant PC/ABS Alloy Features:UL V-0 @ 3.2mmExcellent balance propertiesGood low temperature resistanceGood normal/low temperature impact strengthGood surfaceApplications:ControllerPlugSocketShell of ammeterInformation .. |
|||
Izod Impact, Notched | 3.80 J/cm @Thickness 3.20 mm, Temperature -10.0 °C |
7.12 ft-lb/in @Thickness 0.126 in, Temperature 14.0 °F |
ASTM D256 |
Kingfa JH960 6100 Non-halogenated Flame Retardant PC/ABS Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent mechanical propertiesChemical resistanceHydrolysis resistanceDrop down resistantSuper high flow ability, suit for thin w.. |
|||
Izod Impact, Notched | 3.80 J/cm @Thickness 3.20 mm, Temperature -10.0 °C |
7.12 ft-lb/in @Thickness 0.126 in, Temperature 14.0 °F |
ASTM D256 |
Kingfa JH960 6111 Non-halogenated Flame Retardant PC/ABS Alloy Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent mechanical propertiesHigh heat resistanceChemical resistance, hydrolysis resistanceGood paint adhesionHigh flow ability,.. |
|||
Izod Impact, Notched | 3.80 J/cm @Thickness 3.20 mm, Temperature -10.0 °C |
7.12 ft-lb/in @Thickness 0.126 in, Temperature 14.0 °F |
ASTM D256 |
Kingfa JH960 6300 Non-halogenated Flame Retardant PC/ABS Alloy Features:Halogen free flame retardant, V-0/1.5mm5VB/1.6mm, 5VA/3.2mmExcellent balance propertiesHigh heat resistanceGood chemical resistanceGood hydrolysis resistanceSuit for paint and electo-platin.. |
|||
Izod Impact, Notched | 3.80 J/cm @Thickness 3.20 mm, Temperature -10.0 °C |
7.12 ft-lb/in @Thickness 0.126 in, Temperature 14.0 °F |
ASTM D256 |
Kingfa JH960 6610 Non-halogenated Flame Retardant PC/ABS Alloy Features:Halogen free flame retardant, V-0/1.5mmExcellent balance propertiesHigh heat resistanceGood chemical resistanceGood hydrolysis resistanceSuit for paint and electo-platingDrop down resistanc.. |
|||
Izod Impact, Notched | 3.80 J/cm @Temperature 0.000 °C |
7.12 ft-lb/in @Temperature 32.0 °F |
ASTM D 638 |
Cossa Polimeri ESTADIENE 4009 Acrylonitrile Butadiene Styrene ABS with high impact resistanceHigh impact resistance at low temperature, high gloss, good processabilityInformation provided by Cossa Polimeri S.r.l. |