Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 1.90 GPa @Temperature 100 °C |
276 ksi @Temperature 212 °F |
ISO 527 |
BASF Ultrason® P 3010 PPSU Unreinforced Polyphenylsulfone Description: Medium viscosity injection-molding and extrusion grade with good toughness and chemical resistance (stress crack resistance), resistant against superheated steam. The property profile m.. |