Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 9.00 GPa @Temperature 120 °C |
1310 ksi @Temperature 248 °F |
ISO 527 |
BASF Ultrason S 2010 G6 30% Glass Filled PSU Ultrason S 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength. |
|||
Modulus of Elasticity | 9.00 GPa @Temperature 20.0 °C |
1310 ksi @Temperature 68.0 °F |
ISO 527 |
BASF Ultrason S 2010 G6 30% Glass Filled PSU Ultrason S 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength. |