Mechanical Properties Metric English Comments
Modulus of Elasticity 9.00 GPa

@Temperature 120 °C
1310 ksi

@Temperature 248 °F
ISO 527
BASF Ultrason S 2010 G6 30% Glass Filled PSU
Ultrason S 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength.
Modulus of Elasticity 9.00 GPa

@Temperature 20.0 °C
1310 ksi

@Temperature 68.0 °F
ISO 527
BASF Ultrason S 2010 G6 30% Glass Filled PSU
Ultrason S 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength.