Polymer Property : Modulus of Elasticity = 1700 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 11.7 GPa

@Thickness 1.57 mm
1700 ksi

@Thickness 0.0620 in
CW; ASTM D229
Industrial Laminates/Norplex NP193E Synthetic Fabric
Description: 17 oz. aramid and "soft glass" fibers are combined to make a fabric that is stronger than pure aramid and less abrasive than glass fabrics. This material is impregnated with a high temp..
Modulus of Elasticity 11.7 GPa

@Thickness 1.57 mm
1700 ksi

@Thickness 0.0620 in
LW; ASTM D229
Industrial Laminates/Norplex NP320 Cotton Fabric
Description: Fine weave (less than 4 ounce/square yard) cotton fabric commonly called linen, combined with phenolic resin to provide better machining than NP310. For smaller and more intricate shape..
Modulus of Elasticity 11.7 GPa

@Thickness 1.57 mm
1700 ksi

@Thickness 0.0620 in
LW; ASTM D229
Industrial Laminates/Norplex NP342 Cotton Fabric
Description: Fine weave canvas phenolic material with fabric construction weight intermediate to NP310 and NP320. Designed for better machining than grade NP310 and lower cost than NP320.Thickness T..
Modulus of Elasticity 11.7 GPa

@Thickness 1.57 mm
1700 ksi

@Thickness 0.0620 in
CW; ASTM D229
Industrial Laminates/Norplex NP509 Glass Fabric
Description: Woven glass fabric, melamine resin laminate. Very hard, flame resistant, machining grade with excellent electrical properties in high humidity conditions. High physical strength and exc..