Polymer Property : Modulus of Elasticity = 27800 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 192 GPa

@Temperature 410 °C
27800 ksi

@Temperature 770 °F
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 538°C (1000°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man..
Modulus of Elasticity 192 GPa

@Temperature 410 °C
27800 ksi

@Temperature 770 °F
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 704°C (1300°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man..
Modulus of Elasticity 192 GPa

@Temperature 410 °C
27800 ksi

@Temperature 770 °F
Haynes Hastelloy® N, 1.6 mm sheet, heat treated at 1175°C, welded and tested as welded
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man..
Modulus of Elasticity 192 GPa

@Temperature 410 °C
27800 ksi

@Temperature 770 °F
Haynes Hastelloy® N, weld metal as welded
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man..
Modulus of Elasticity 192 GPa

@Temperature 410 °C
27800 ksi

@Temperature 770 °F
Haynes Hastelloy® N, weld metal, aged 500 hours at 649°C (1200°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the man..
Modulus of Elasticity 192 GPa

@Temperature 400 °C
27800 ksi

@Temperature 752 °F
Haynes Waspaloyâ„¢ alloy, sheet
Age-hardenable superalloy with very good strength at temperatures up 980°C (1800°F), can be cold-formed in the annealed condition, may also be hot formed at 1040°C (1900°F) and above, go..
Modulus of Elasticity 192 GPa

@Temperature 199 °C
27800 ksi

@Temperature 390 °F
EDRO #7 Shock Resistant S7 Tool Steel
EDRO #7™ is a chromium-molybdenum steel characterized by: high toughness, good wear resistance, high impact resistance, good through hardening properties, good machinability, and good dimensional s..
Modulus of Elasticity 192 GPa

@Temperature 200 °C
27800 ksi

@Temperature 392 °F
Hardened and tempered to 60-62 HRC
Bohler-Uddeholm UDDEHOLM Caldie Plastic Mold Tool Steel
Description: Uddeholm Caldie is a chromium-molybdenumvanadium alloyed tool steel.Uddeholm Caldie which is characterized by:Very good chipping and cracking resistanceGood wear resistanceHigh hardness..
Modulus of Elasticity 192 GPa

@Temperature 410 °C
27800 ksi

@Temperature 770 °F
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 593°C (1100°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..
Modulus of Elasticity 192 GPa

@Temperature 410 °C
27800 ksi

@Temperature 770 °F
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 760°C (1400°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..
Modulus of Elasticity 192 GPa

@Temperature 410 °C
27800 ksi

@Temperature 770 °F
Haynes Hastelloy® N, 1.6 mm sheet, aged 128 hours at 815°C (1500°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..
Modulus of Elasticity 192 GPa

@Temperature 410 °C
27800 ksi

@Temperature 770 °F
Haynes Hastelloy® N, 1.6 mm sheet, heat treated at 1175°C, rapid air cooled
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..
Modulus of Elasticity 192 GPa

@Temperature 410 °C
27800 ksi

@Temperature 770 °F
Haynes Hastelloy® N, 1.14 mm sheet, aged 10000 hours at 649°C (1200°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..
Modulus of Elasticity 192 GPa

@Temperature 410 °C
27800 ksi

@Temperature 770 °F
Haynes Hastelloy® N, 1.14 mm sheet, heat treated at 1149°C (2100°F)
Applications include containers for molten fluoride salts. Good oxidation resistance to hot fluoride salts at 705-870°C (1300-1600°F), good oxidation resistance in air.Data provided by the manufac..