Description: Uddeholm Caldie is a chromium-molybdenumvanadium alloyed tool steel.Uddeholm Caldie which is characterized by:Very good chipping and cracking resistanceGood wear resistanceHigh hardness (>60 HRC) after high temperature temperingGood dimensional stability in heat treatment and in serviceExcellent through-hardening propertiesGood machinability and grindabilityExcellent polishabilityGood surface treatment propertiesGood resistance to tempering backVery good WEDM propertiesApplications: Uddeholm Caldie is suitable for short to medium run tooling where chipping and/or cracking are the predominant failure mechanisms and where a high compressive strength (hardness of over 60 HRC) is necessary. This makes Uddeholm Caldie an excellent problem solver for severe cold work applications where the combination of a hardness above 60 HRC and a high cracking resistance is of utmost importance e.g. as in the blanking and forming of ultra high strength steel sheets. Uddeholm Caldie is also very suitable as a substrate steel for applications where surface coatings are desirable or necessaryCold Work Applications:Blanking applications where high ductility and toughness are needed to prevent chipping/crackingCold forging and forming operations where a high compressive strength combined with good resistance to chipping/cracking are necessaryMachine knivesThread rolling diesSubstrate for surface coatings
Physical Properties Metric English Comments
Density 7.82 g/cc
0.283 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 215
215
Soft annealed
Hardness, Rockwell C 60 - 62
60 - 62
typical range of use after hardening/tempering
Modulus of Elasticity 180 GPa

@Temperature 400 °C
26100 ksi

@Temperature 752 °F
Hardened and tempered to 60-62 HRC
192 GPa

@Temperature 200 °C
27800 ksi

@Temperature 392 °F
Hardened and tempered to 60-62 HRC
213 GPa

@Temperature 20.0 °C
30900 ksi

@Temperature 68.0 °F
Hardened and tempered to 60-62 HRC
Compressive Strength 2230 - 2430 MPa
323000 - 352000 psi
Rc0.2; varies with tempering. This range is for HRC between 58 and 61.
Thermal Properties Metric English Comments
CTE, linear 11.6 µm/m-°C

@Temperature 20.0 - 200 °C
6.44 µin/in-°F

@Temperature 68.0 - 392 °F
Hardened and tempered to 60-62 HRC
12.4 µm/m-°C

@Temperature 20.0 - 400 °C
6.89 µin/in-°F

@Temperature 68.0 - 752 °F
Hardened and tempered to 60-62 HRC
Specific Heat Capacity 0.460 J/g-°C
0.110 BTU/lb-°F
Hardened and tempered to 60-62 HRC
Thermal Conductivity 24.0 W/m-K

@Temperature 200 °C
167 BTU-in/hr-ft²-°F

@Temperature 392 °F
Hardened and tempered to 60-62 HRC
28.0 W/m-K

@Temperature 400 °C
194 BTU-in/hr-ft²-°F

@Temperature 752 °F
Hardened and tempered to 60-62 HRC
Component Elements Properties Metric English Comments
Carbon, C 0.70 %
0.70 %
Chromium, Cr 5.0 %
5.0 %
Iron, Fe 90.8 %
90.8 %
As Balance
Manganese, Mn 0.50 %
0.50 %
Molybdenum, Mo 2.3 %
2.3 %
Silicon, Si 0.20 %
0.20 %
Vanadium, V 0.50 %
0.50 %
Users viewing this material also viewed the following: