Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Total Energy | 53.8 J/cm @Temperature 23.0 °C |
0.101 ft-lb/mil @Temperature 73.4 °F |
Procedure A, C.125; ASTM D4226 |
PolyOne Geon™ Vinyl Rigid Extrusion L1101 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Dart Drop Total Energy | 53.8 J/cm @Temperature 23.0 °C |
0.101 ft-lb/mil @Temperature 73.4 °F |
Procedure A, C.125; ASTM D4226 |
PolyOne Geon™ Vinyl Cellular E2519 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Physical properties were measured on non-foamed profiles. Measured density of an extruded 1 thick free foamed part was 0.70 gms/cc at a 360 deg.F melt temperature.Information provided by PolyO.. |
|||
Dart Drop Total Energy | 53.8 J/cm @Temperature 23.0 °C |
0.101 ft-lb/mil @Temperature 73.4 °F |
Procedure B, C.125; ASTM D4226 |
PolyOne Geon™ Vinyl Cellular E2519 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: Physical properties were measured on non-foamed profiles. Measured density of an extruded 1 thick free foamed part was 0.70 gms/cc at a 360 deg.F melt temperature.Information provided by PolyO.. |
|||
Dart Drop Total Energy | 53.8 J/cm @Temperature 23.0 °C |
0.101 ft-lb/mil @Temperature 73.4 °F |
Procedure A, C.125; ASTM D4226 |
PolyOne Geon™ Vinyl Dry Blend E6530 Polyvinyl Chloride, Rigid (PVC, Rigid) Interior application for thick & thin gauge profile application.Information provided by PolyOne |