Mechanical Properties Metric English Comments
Dart Drop Total Energy 53.8 J/cm

@Temperature 23.0 °C
0.101 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
PolyOne Geon™ Vinyl Rigid Extrusion L1101 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Dart Drop Total Energy 53.8 J/cm

@Temperature 23.0 °C
0.101 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
PolyOne Geon™ Vinyl Cellular E2519 Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: Physical properties were measured on non-foamed profiles. Measured density of an extruded 1 thick free foamed part was 0.70 gms/cc at a 360 deg.F melt temperature.Information provided by PolyO..
Dart Drop Total Energy 53.8 J/cm

@Temperature 23.0 °C
0.101 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
PolyOne Geon™ Vinyl Cellular E2519 Polyvinyl Chloride, Rigid (PVC, Rigid)
Note: Physical properties were measured on non-foamed profiles. Measured density of an extruded 1 thick free foamed part was 0.70 gms/cc at a 360 deg.F melt temperature.Information provided by PolyO..
Dart Drop Total Energy 53.8 J/cm

@Temperature 23.0 °C
0.101 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
PolyOne Geon™ Vinyl Dry Blend E6530 Polyvinyl Chloride, Rigid (PVC, Rigid)
Interior application for thick & thin gauge profile application.Information provided by PolyOne