Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop Total Energy | 165 J/cm @Temperature 23.0 °C |
0.309 ft-lb/mil @Temperature 73.4 °F |
Procedure B, C.125; ASTM D4226 |
PolyOne Geon™ Vinyl Rigid Extrusion L9630 Polyvinyl Chloride, Rigid (PVC, Rigid) Product can meet UL-94V-0. Material passed V-0 @ 1.5mm in screening test at PDI.Information provided by PolyOne |