Polymer Property : Dart Drop Total Energy = 165 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop Total Energy 165 J/cm

@Temperature 23.0 °C
0.309 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
PolyOne Geon™ Vinyl Rigid Extrusion L9630 Polyvinyl Chloride, Rigid (PVC, Rigid)
Product can meet UL-94V-0. Material passed V-0 @ 1.5mm in screening test at PDI.Information provided by PolyOne