Mechanical Properties Metric English Comments
Dart Drop Total Energy 52.0 J/cm

@Temperature 23.0 °C
0.0974 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
PolyOne Geon™ Vinyl Rigid Extrusion 87547 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Dart Drop Total Energy 52.0 J/cm

@Temperature 23.0 °C
0.0974 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
PolyOne Geon™ Vinyl Rigid Extrusion 87548 AS Polyvinyl Chloride, Rigid (PVC, Rigid)
A transparent PVC profile compound, with reduced surface resistivity, resulting in unlikely attraction and adhesion of dust. Actual results on surface resistivity = 1.3x10^15.Information provided by..
Dart Drop Total Energy 52.0 J/cm

@Temperature 23.0 °C
0.0974 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
PolyOne Geon™ Vinyl Rigid Extrusion 87548 Polyvinyl Chloride, Rigid (PVC, Rigid)
A transparent PVC profile compound, with inherent water clear optical characteristics.Information provided by PolyOne
Dart Drop Total Energy 52.0 J/cm

@Temperature 23.0 °C
0.0974 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
PolyOne Geon™ Vinyl Rigid Extrusion 87554 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Dart Drop Total Energy 52.0 J/cm

@Temperature 23.0 °C
0.0974 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
PolyOne Geon™ Vinyl Rigid Extrusion 87555 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Dart Drop Total Energy 52.0 J/cm

@Temperature 23.0 °C
0.0974 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
PolyOne Geon™ Vinyl Rigid Extrusion 87556 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Dart Drop Total Energy 52.0 J/cm

@Temperature 23.0 °C
0.0974 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
PolyOne Geon™ Vinyl Rigid Extrusion L7801 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Dart Drop Total Energy 52.0 J/cm

@Temperature 23.0 °C
0.0974 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
PolyOne Geon™ HTX Ultra LA436G Black 2880 Polyvinyl Chloride Alloy (PVC Alloy)
Higher gloss, wider processing window version of Geon HTX Ultra LA426G.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical properties measured on LA436G Black 2880...