Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 73.5 MPa @Strain 1.05 %, Temperature -20.0 °C |
10700 psi @Strain 1.05 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9320 NC010 PBT+SAN
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9320 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. I.. |
|||
Tensile Stress | 73.5 MPa @Strain 1.20 %, Temperature 23.0 °C |
10700 psi @Strain 1.20 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK603 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Crastin SK603 NC010 is a 20% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Tensile Stress | 73.5 MPa @Strain 12.0 %, Temperature 0.000 °C |
10700 psi @Strain 12.0 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 527UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized Medium Viscosity Acetal HomopolymerDelrin 527UV NC010 is a medium viscosity acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has improvem.. |