Tensile Stress 73.5 MPa

@Strain 1.05 %,
Temperature -20.0 °C
10700 psi

@Strain 1.05 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9320 NC010 PBT+SAN  (Unverified Data**)
20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9320 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. I..
Tensile Stress 73.5 MPa

@Strain 1.20 %,
Temperature 23.0 °C
10700 psi

@Strain 1.20 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK603 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
20% Glass Reinforced Polybutylene Terephthalate Crastin SK603 NC010 is a 20% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P..
Tensile Stress 73.5 MPa

@Strain 12.0 %,
Temperature 0.000 °C
10700 psi

@Strain 12.0 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 527UV NC010 Acetal (POM)  (Unverified Data**)
UV Stabilized Medium Viscosity Acetal HomopolymerDelrin 527UV NC010 is a medium viscosity acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has improvem..