Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 1.53 MPa @Strain 100 % |
222 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® A9955H TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Tensile Stress | 1.53 MPa @Strain 100 % |
222 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P2750 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 1.53 MPa @Strain 0.500 %, Temperature 90.0 °C |
222 psi @Strain 0.500 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1610 BK387 Nylon 1010
(Unverified Data**) Plasticized Toughened Renewably Sourced Polyamide 1010 Developed for Extrusion Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 1.53 MPa @Strain 6.00 %, Temperature 90.0 °C |
222 psi @Strain 6.00 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process.. |