Mechanical Properties Metric English Comments
Tensile Stress 1.65 MPa

@Strain 100 %
239 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® A9950C TPE, ABS/PC Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform..
Tensile Stress 1.65 MPa

@Strain 100 %
239 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® D6855 TPE, Extruded
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from..
Tensile Stress 1.65 MPa

@Strain 100 %
239 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® N8960 TPE, Nylon Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Auto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInformation from Alliance Polymers & Se..
Tensile Stress 1.65 MPa

@Strain 300 %
239 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P2645 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 1.65 MPa

@Strain 300 %
239 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P2840 TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 1.65 MPa

@Strain 300 %,
Temperature 23.0 °C
239 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7630-1 (Natural) Thermoplastic Elastomer (TPE)
Dynaflex™ G7630-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhe..
Tensile Stress 1.65 MPa

@Strain 300 %,
Temperature 23.0 °C
239 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7630-9 (Black) Thermoplastic Elastomer (TPE)
Dynaflex™ G7630-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. *Made with Kraton® Polymer - Non..
Tensile Stress 1.65 MPa

@Strain 100 %,
Temperature 23.0 °C
239 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412