Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 1.65 MPa @Strain 100 % |
239 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® A9950C TPE, ABS/PC Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform.. |
|||
Tensile Stress | 1.65 MPa @Strain 100 % |
239 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® D6855 TPE, Extruded Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from.. |
|||
Tensile Stress | 1.65 MPa @Strain 100 % |
239 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® N8960 TPE, Nylon Overmold Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Auto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInformation from Alliance Polymers & Se.. |
|||
Tensile Stress | 1.65 MPa @Strain 300 % |
239 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P2645 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 1.65 MPa @Strain 300 % |
239 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P2840 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 1.65 MPa @Strain 300 %, Temperature 23.0 °C |
239 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7630-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7630-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhe.. |
|||
Tensile Stress | 1.65 MPa @Strain 300 %, Temperature 23.0 °C |
239 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7630-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7630-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. *Made with Kraton® Polymer - Non.. |
|||
Tensile Stress | 1.65 MPa @Strain 100 %, Temperature 23.0 °C |
239 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G2709-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2709-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone/UV Stability - Overmol.. |