Mechanical Properties Metric English Comments
Tensile Stress 71.64 MPa

@Strain 2.62 %,
Temperature 90.0 °C
10390 psi

@Strain 2.62 %,
Temperature 194 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 73G30HSL NC010 Nylon 6  (Unverified Data**)
30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL NC010 is a 30% glass fiber reinforced heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performan..
Tensile Stress 71.62 MPa

@Strain 0.840 %,
Temperature 40.0 °C
10390 psi

@Strain 0.840 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 54G35HSLR BK031 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G35HSLR BK031 is a 35% glass reinforced toughened heat stabilized hydrolysis resistant high performance polyamide resin. It i..