Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 76.17 MPa @Strain 0.800 %, Temperature -20.0 °C |
11050 psi @Strain 0.800 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 935SUV BK593 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced UV Stabilized Polyethylene Terephthalate Rynite 935SUV BK593 is a 35% glass fiber /mineral reinforced UV stabilized modified polyethylene terephthalate resin with low warpage de.. |
|||
Tensile Stress | 76.16 MPa @Strain 9.43 %, Temperature 150 °C |
11050 psi @Strain 9.43 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 53G50HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**) 50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR NC010 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve.. |
|||
Tensile Stress | 76.21 MPa @Strain 3.90 %, Temperature 150 °C |
11050 psi @Strain 3.90 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTN52G35HSL BK083 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin that can be molded in water heated m.. |