Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 77.1 MPa @Strain 21.4 %, Temperature 0.000 °C |
11200 psi @Strain 21.4 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging.. |
|||
Tensile Stress | 77.2 MPa @Strain 9.60 %, Temperature -40.0 °C |
11200 psi @Strain 9.60 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500T NC010 Acetal (POM)
(Unverified Data**) Toughened Medium Viscosity Acetal Homopolymer Delrin 500T NC010 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri.. |
|||
Tensile Stress | 77.5 MPa @Strain 10.8 %, Temperature 0.000 °C |
11200 psi @Strain 10.8 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500TL is a medium viscosity acetal homopolymer resin containing 1.5% Teflon PTFE Micropowder. It is desi.. |
|||
Tensile Stress | 77.5 MPa @Strain 10.8 %, Temperature 0.000 °C |
11200 psi @Strain 10.8 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG500TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact ApplicationsDelrin FG500TL medium viscosity acetal homopolymer resin containing 1.5%.. |
|||
Tensile Stress | 77.0 MPa @Strain 0.700 %, Temperature -40.0 °C |
11200 psi @Strain 0.700 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G33HS1L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G33HS1L NC010 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor.. |
|||
Tensile Stress | 77.1 MPa @Strain 5.00 %, Temperature 0.000 °C |
11200 psi @Strain 5.00 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Improved Processing Delrin 500P is a medium viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical .. |
|||
Tensile Stress | 77.0 MPa @Strain 0.860 %, Temperature -20.0 °C |
11200 psi @Strain 0.860 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® GW520CS NC010 Polyethylene Terephthalate (PET) 20% Glass Reinforced Flame Retardant Polyethylene Terephthalate with Improved Glow Wire Performance Rynite GW520CS NC010 is a 20% glass fiber reinforced flame retardant color stabilized modified pol.. |