Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 79.11 MPa @Strain 0.600 %, Temperature 0.000 °C |
11470 psi @Strain 0.600 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G50HSLA BK416 Nylon 6
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G50HSLA BK416 is a 50% glass fiber reinforced heat stabilized lubricated polyamide 6 resin for injection molding. It has an excellent surface.. |
|||
Tensile Stress | 79.11 MPa @Strain 1.75 %, Temperature 40.0 °C |
11470 psi @Strain 1.75 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66
(Unverified Data**) 25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR70G25V0 NC010 is a 25% glass fiber reinforced heat stabilized flame retardant polyamide 66 resin for injection molding.Information provided .. |