Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 79.11 MPa

@Strain 0.600 %,
Temperature 0.000 °C
11470 psi

@Strain 0.600 %,
Temperature 32.0 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 73G50HSLA BK416 Nylon 6  (Unverified Data**)
50% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G50HSLA BK416 is a 50% glass fiber reinforced heat stabilized lubricated polyamide 6 resin for injection molding. It has an excellent surface..
Tensile Stress 79.11 MPa

@Strain 1.75 %,
Temperature 40.0 °C
11470 psi

@Strain 1.75 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66  (Unverified Data**)
25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR70G25V0 NC010 is a 25% glass fiber reinforced heat stabilized flame retardant polyamide 66 resin for injection molding.Information provided ..