Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 12.07 MPa @Strain 4.64 %, Temperature 90.0 °C |
1751 psi @Strain 4.64 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® 6129 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection MoldingInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 12.07 MPa @Strain 4.64 %, Temperature 90.0 °C |
1751 psi @Strain 4.64 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® 6130 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin 6130 NC010 is an unreinforced medium high viscosity polybutylene terephthalate resin for .. |
|||
Tensile Stress | 12.07 MPa @Strain 1.10 %, Temperature 100 °C |
1751 psi @Strain 1.10 %, Temperature 212 °F |
ISO 11403-1/-2 |
DuPont Performance Polymers Delrin® 511P BK402 Acetal Homopolymer Delrin® 511P is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Information provided .. |
|||
Tensile Stress | 12.07 MPa @Strain 130.96 %, Temperature 120 °C |
1751 psi @Strain 130.96 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 8238 Polyester Elastomer TPC-ET
(Unverified Data**) 82 Shore D Standard Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 12.07 MPa @Strain 0.600 %, Temperature 60.0 °C |
1751 psi @Strain 0.600 %, Temperature 140 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® FR7026V0F BK001 Nylon 66
(Unverified Data**) Zytel® FR7026V0F BK001 is a flame retardant heat stabilized polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuP.. |
|||
Tensile Stress | 12.07 MPa @Strain 213.35 %, Temperature 150 °C |
1751 psi @Strain 213.35 %, Temperature 302 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8441 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 12.07 MPa @Strain 24.82 %, Temperature 60.0 °C |
1751 psi @Strain 24.82 %, Temperature 140 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8441 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |