Mechanical Properties Metric English Comments
Tensile Stress 12.07 MPa

@Strain 4.64 %,
Temperature 90.0 °C
1751 psi

@Strain 4.64 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® 6129 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection MoldingInformation provided by DuPont Performance Polymers
Tensile Stress 12.07 MPa

@Strain 4.64 %,
Temperature 90.0 °C
1751 psi

@Strain 4.64 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® 6130 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin 6130 NC010 is an unreinforced medium high viscosity polybutylene terephthalate resin for ..
Tensile Stress 12.07 MPa

@Strain 1.10 %,
Temperature 100 °C
1751 psi

@Strain 1.10 %,
Temperature 212 °F
ISO 11403-1/-2
DuPont Performance Polymers Delrin® 511P BK402 Acetal Homopolymer
Delrin® 511P is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Information provided ..
Tensile Stress 12.07 MPa

@Strain 130.96 %,
Temperature 120 °C
1751 psi

@Strain 130.96 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 8238 Polyester Elastomer TPC-ET  (Unverified Data**)
82 Shore D Standard Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 12.07 MPa

@Strain 0.600 %,
Temperature 60.0 °C
1751 psi

@Strain 0.600 %,
Temperature 140 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® FR7026V0F BK001 Nylon 66  (Unverified Data**)
Zytel® FR7026V0F BK001 is a flame retardant heat stabilized polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuP..
Tensile Stress 12.07 MPa

@Strain 213.35 %,
Temperature 150 °C
1751 psi

@Strain 213.35 %,
Temperature 302 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8441 BK316 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers
Tensile Stress 12.07 MPa

@Strain 24.82 %,
Temperature 60.0 °C
1751 psi

@Strain 24.82 %,
Temperature 140 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8441 BK316 Polyester Elastomer TPC-ET  (Unverified Data**)