Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 12.1 MPa @Strain 100 % |
1750 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® F7895 TPE, Fire Retardant Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Auto PartsSealsWire & Cable ElectronicsInformation from Alliance Polymers & Services, Distributor of Nantong Elastome.. |
|||
Tensile Stress | 12.1 MPa @Strain 0.48467 %, Temperature 100 °C |
1750 psi @Strain 0.48467 %, Temperature 212 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 510GR NC000 Acetal Homopolymer
(Unverified Data**) Delrin® 510GR is a 10% glass reinforced acetal homopolymer for injection molding. It has high strength, stiffness, and high deflection temperature and excellent creep resistance.Information provide.. |
|||
Tensile Stress | 12.1 MPa @Strain 0.250 %, Temperature 0.000 °C |
1750 psi @Strain 0.250 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK601 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 10% Glass Reinforced Polybutylene Terephthalate Crastin SK601 NC010 is a 10% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Tensile Stress | 12.1 MPa @Strain 50.0 % |
1750 psi @Strain 50.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® HTR237BG BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR237BG is designed for blow molding or processing techniques requiring high viscosity. It has nominal dur.. |
|||
Tensile Stress | 12.1 MPa @Strain 0.520 %, Temperature 60.0 °C |
1750 psi @Strain 0.520 %, Temperature 140 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |