Mechanical Properties Metric English Comments
Tensile Stress 12.1 MPa

@Strain 100 %
1750 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® F7895 TPE, Fire Retardant
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Auto PartsSealsWire & Cable ElectronicsInformation from Alliance Polymers & Services, Distributor of Nantong Elastome..
Tensile Stress 12.1 MPa

@Strain 0.48467 %,
Temperature 100 °C
1750 psi

@Strain 0.48467 %,
Temperature 212 °F
ISO 527
DuPont Performance Polymers Delrin® 510GR NC000 Acetal Homopolymer  (Unverified Data**)
Delrin® 510GR is a 10% glass reinforced acetal homopolymer for injection molding. It has high strength, stiffness, and high deflection temperature and excellent creep resistance.Information provide..
Tensile Stress 12.1 MPa

@Strain 0.250 %,
Temperature 0.000 °C
1750 psi

@Strain 0.250 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK601 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
10% Glass Reinforced Polybutylene Terephthalate Crastin SK601 NC010 is a 10% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P..
Tensile Stress 12.1 MPa

@Strain 50.0 %
1750 psi

@Strain 50.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® HTR237BG BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
45 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR237BG is designed for blow molding or processing techniques requiring high viscosity. It has nominal dur..
Tensile Stress 12.1 MPa

@Strain 0.520 %,
Temperature 60.0 °C
1750 psi

@Strain 0.520 %,
Temperature 140 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT  (Unverified Data**)