Mechanical Properties Metric English Comments
Tensile Stress 9.03 MPa

@Strain 300 %
1310 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® D6890 TPE, Extruded
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from..
Tensile Stress 9.03 MPa

@Strain 300 %
1310 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® D6785 TPE, Extruded
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsSealsWire & Cable ElectronicsMedical DevicesInformation from..
Tensile Stress 9.06 MPa

@Strain 7.90 %,
Temperature 150 °C
1310 psi

@Strain 7.90 %,
Temperature 302 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® S600F20 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provi..
Tensile Stress 9.06 MPa

@Strain 7.90 %,
Temperature 150 °C
1310 psi

@Strain 7.90 %,
Temperature 302 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® S600F20UV WT660 Polybutylene Terephthalate (PBT)
Unreinforced UV Stabilized Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provided..
Tensile Stress 9.04 MPa

@Strain 56.83 %,
Temperature 90.0 °C
1310 psi

@Strain 56.83 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers
Tensile Stress 9.01 MPa

@Strain 144.39 %,
Temperature 100 °C
1310 psi

@Strain 144.39 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT  (Unverified Data**)
Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 9.04 MPa

@Strain 0.820 %,
Temperature 150 °C
1310 psi

@Strain 0.820 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70K20HSL NC010 Nylon 66  (Unverified Data**)
Kevlar® Fiber Reinforced Heat Stabilized Polyamide 66 Zytel 70K20HSL NC010 is a heat stabilized PA66 resin modified with Kevlar aramid fiber for excellent wear resistance.Information provided by Du..
Tensile Stress 9.00 MPa

@Strain 0.349 %,
Time 360000 sec
1310 psi

@Strain 0.349 %,
Time 100 hour
50%RH; isochronous; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 80G14A NC010A Nylon 66  (Unverified Data**)
14% Glass Reinforced Toughened Polyamide 66 Zytel 80G14A NC010A is a 14% glass fiber reinforced toughened high flow polyamide 66 resin. It offers outstanding performance in injection molding applica..
Tensile Stress 9.02 MPa

@Strain 0.100 %,
Temperature -40.0 °C
1310 psi

@Strain 0.100 %,
Temperature -40.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FR52G20NH NC010 Polyphthalamide (PPA)  (Unverified Data**)
20% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G20NH NC010 is a 20% glass reinforced flame retardant lubricated high performance polyamide resin. It..
Tensile Stress 9.05 MPa

@Strain 0.240 %,
Temperature 150 °C
1310 psi

@Strain 0.240 %,
Temperature 302 °F
50%RH; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS90G30DR BK099 Nylon 66  (Unverified Data**)
Zytel® PLS90G30DR BK099 is a 30% glass reinforced PA66 nylon resin having superior resistance to hot engine coolant. It is particularly suitable for automotive Radiator End Tanks and other parts in..
Tensile Stress 9.06 MPa

@Strain 5.00 %,
Temperature 23.0 °C
1310 psi

@Strain 5.00 %,
Temperature 73.4 °F
ISO 527
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET  (Unverified Data**)
Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac..
Tensile Stress 9.00 MPa

@Strain 50.0 %
1310 psi

@Strain 50.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc..
Tensile Stress 9.00 MPa

@Strain 27.59 %,
Temperature 90.0 °C
1310 psi

@Strain 27.59 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET  (Unverified Data**)
55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc..
Tensile Stress 9.03 MPa

@Strain 100 %
1310 psi

@Strain 100 %
ASTM D412
Alliance Polymers Zythane™ 4045D Thermoplastic Polyurethane Elastomer
Zythane™ 4045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tensile Stress 9.03 MPa

@Strain 100 %
1310 psi

@Strain 100 %
ASTM D412
Alliance Polymers Zythane™ 5045D Thermoplastic Polyurethane Elastomer
Zythane™ 5045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tensile Stress >= 9.00 MPa

@Strain 300 %
>= 1310 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 282A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech
Tensile Stress >= 9.00 MPa

@Strain 100 %
>= 1310 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 590A Polyether-based TPU
Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech
Tensile Stress >= 9.00 MPa

@Strain 100 %
>= 1310 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 795A PCL TPU
Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech
Tensile Stress >= 9.00 MPa

@Strain 100 %
>= 1310 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 395A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech
Tensile Stress >= 9.00 MPa

@Strain 100 %
>= 1310 psi

@Strain 100 %
ISO 37
Austin Novel Materials Texalan® 398A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech
Tensile Stress >= 9.00 MPa

@Strain 300 %
>= 1310 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 385A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech
Tensile Stress >= 9.00 MPa

@Strain 300 %
>= 1310 psi

@Strain 300 %
ISO 37
Austin Novel Materials Texalan® 785A PCL TPU
Description: Good abrasion resistance, tensile strength, oil resistance and heat resistance which can be used in mechanic parts and various industry parts.Information from Dawnentech