Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 91.43 MPa @Strain 1.30 %, Temperature 40.0 °C |
13260 psi @Strain 1.30 %, Temperature 104 °F |
ISO 527 |
DuPont Performance Polymers Crastin® SK608 BK509 PBT
(Unverified Data**) Crastin® SK608 BK509 is a 45% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 91.45 MPa @Strain 1.21 %, Temperature 23.0 °C |
13260 psi @Strain 1.21 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5330HFS BK591 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for inject.. |
|||
Tensile Stress | 91.45 MPa @Strain 1.21 %, Temperature 23.0 °C |
13260 psi @Strain 1.21 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5330HFS NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate with Improved Processing Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for in.. |
|||
Tensile Stress | 91.43 MPa @Strain 1.30 %, Temperature 40.0 °C |
13260 psi @Strain 1.30 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK608 BK509 Polybutylene Terephthalate (PBT)
(Unverified Data**) 45% Glass Reinforced Polybutylene Terephthalate Crastin SK608 BK509 is a 45% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du.. |