Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 92.13 MPa @Strain 0.950 %, Temperature 0.000 °C |
13360 psi @Strain 0.950 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 54G35HSLR BK031 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced Toughened PPA High Performance Polyamide Zytel HTN54G35HSLR BK031 is a 35% glass reinforced toughened heat stabilized hydrolysis resistant high performance polyamide resin. It i.. |